window._bd_share_config={"common":{"bdSnsKey":{},"bdText":"","bdMini":"2","bdPic":"","bdStyle":"0","bdSize":"16"},"share":{},"image":{"viewList":["qzone","tsina","tqq","renren","weixin"],"viewText":"分享到:","viewSize":"16"},"selectShare":{"bdContainerClass":null,"bdSelectMiniList":["qzone","tsina","tqq","renren","weixin"]}};with(document)0[(getElementsByTagName('head')[0]||body).appendChild(createElement('script')).src='http://bdimg.share.baidu.com/static/api/js/share.js?v=89860593.js?cdnversion='+~(-new Date()/36e5)];

真空復(fù)膜袋定制廠家—淺談?wù)婵沾鼰岱夂蟠勇N曲的原因?。?/span>

真空袋封口處的靜電:由于外界作用如摩擦或以各種能量如動(dòng)能、位能、熱能、化學(xué)能等的形式作用會使原子的正負(fù)電不平衡。解決辦法:二次加工時(shí),在內(nèi)層PE薄膜中加入3%的衛(wèi)生級抗靜電劑,避免此類問題的發(fā)生。在接顧客定單時(shí),會充分了解客戶的產(chǎn)品特性與自動(dòng)灌裝生產(chǎn)線特點(diǎn),做到有的放矢,更好地滿足客戶要求。


       真空袋熱封后袋子為什么會翹曲呢?原因如下:

       1、復(fù)合膜的厚度不一致;

       2、熱封溫度過高或熱封時(shí)間過長;

       3、在縱向熱封刀部分,復(fù)合膜的運(yùn)行軌跡不平直;

       4、冷卻不充分;

       5、熟化時(shí)間不夠;

       6、表層基材薄膜耐熱性較差;

       7、真空袋復(fù)合過程中復(fù)合基材的張力匹配控制不當(dāng),導(dǎo)致其熟化定型后仍有殘余的應(yīng)力,尤其是復(fù)合膜厚度較薄時(shí)更容易發(fā)生此類故障。


文章名稱:淺談?wù)婵沾鼰岱夂蟠勇N曲的原因!
文章來源:http://muchs.cn/hangye/suliaodai/n67786.html

聲明:本網(wǎng)站發(fā)布的內(nèi)容(圖片、視頻和文字)以用戶投稿、用戶轉(zhuǎn)載內(nèi)容為主,如果涉及侵權(quán)請盡快告知,我們將會在第一時(shí)間刪除。文章觀點(diǎn)不代表本網(wǎng)站立場,如需處理請聯(lián)系客服。電話:028-86922220;郵箱:631063699@qq.com。內(nèi)容未經(jīng)允許不得轉(zhuǎn)載,或轉(zhuǎn)載時(shí)需注明來源: 創(chuàng)新互聯(lián)

塑料袋相關(guān)推薦

我想展現(xiàn)塑料袋信息

加入塑料袋信息推廣

免費(fèi)獲取塑料袋推廣方案
  • 姓名:
  • 電話:
  • 需求:

立即獲取推廣方案

廣告投放
塑料袋咨詢

網(wǎng)站廣告投放說明

提供您的聯(lián)系電話,就能在網(wǎng)上推廣!

1天1元起詳情查看一元廣告投放介紹。

馬上投放我的電話